Understanding Flotation Methods for Polymetallic Sulfide Ore

MineralMiningSolutions2024-08-12Flotation810

Flotation is a commonly used beneficiation method for polymetallic sulfide ores. This article will introduce you to 6 common flotation methods for polymetallic sulfide ores. Here are guides of flotation methods for 6 types of polymetallic sulfide ores.

 Understanding Flotation Methods for Polymetallic Sulfide Ore Equipment production procurement suppliers flotation machines polymetallic ores sulfide equipment applications 第1张

01 Cu-Pb-Zn Flotation

In polymetallic copper-zinc, copper-zinc-sulfur, lead-zinc, lead-zinc-sulfur, copper-lead-zinc and other sulfide ores, the content of copper and lead is generally less than that of zinc. However, the floatability of copper sulfide minerals and galena is better than that of sphalerite, and sphalerite is easily activated by copper sulfide after being inhibited. Therefore, the separation process of suppressing zinc and floating copper and lead is often used.

 Understanding Flotation Methods for Polymetallic Sulfide Ore Equipment production procurement suppliers flotation machines polymetallic ores sulfide equipment applications 第2张

(Cu-Pb-Zn sulfide ore flotation plant)

(1) Cu-Zn preferential flotation

The content of copper in copper-zinc ore is less than that of zinc, but the floatability of copper sulfide minerals is usually better than that of sphalerite, and sphalerite is easily activated after being inhibited. Generally, the method of inhibiting zinc and floating copper is used. In actual production, the priority flotation process is mainly used, followed by the mixed-priority flotation process.

The amount of free copper ions and iron sulfide minerals in copper-zinc ore is the most important problem affecting the flotation and separation of copper-zinc sulfide minerals.

When the content of free copper ions in the copper-zinc-sulfur polymetallic sulfide ore is low, the flotability of sphalerite and pyrite is poor, and the separation is good. Even if no inhibitor is added, good beneficiation indicators can be obtained.

For example, in a copper-zinc-sulfur polymetallic sulfide ore processing plant, the primary copper sulfide accounts for more than 95% of the total copper, and the content of free copper ions is small. Among the zinc minerals, most of the zinc exists in the form of sphalerite, so its floatability is poor. The project uses lime to increase the pH of the pulp, suppresses pyrite, and appropriately reduces the amount of collectors to improve the selectivity of sulfide minerals, thereby realizing the preferential flotation of copper. When zinc is extracted, the lime method is used to inhibit pyrite. Thus, a good beneficiation index was obtained. If the content of free copper ions contained in the ore is large, an inhibitor that reduces free copper ions must be used. At present, the best effect is the sulfurous acid-sodium sulfide inhibition method.

When the content of iron sulfide minerals in the copper-zinc ore is large, the separation becomes difficult. Especially containing a large amount of pyrrhotite, it will accelerate the oxidation of the ore, and various metal ions will be produced after oxidation, which will increase the "unavoidable ions" in the pulp, making it difficult to suppress sphalerite and iron sulfide minerals, increasing the flotation rate. The consumption of reagents leads to more complicated conditions for copper-zinc flotation separation.

For example, the production of a copper mine in China shows that: low-zinc-sulfur ores are better flotated, sphalerite and pyrite are well controlled, and copper, zinc, and sulfur separation indicators are higher; while high-zinc-sulfur ores, pyrite are difficult to inhibition, it is easy to make the copper concentrate with high sulfur content and poor product quality, and at the same time have a serious impact on the separation of zinc and sulfur flotation. At this time, sulfurous acid can be used as an inhibitor to inhibit the activity of pyrite and sphalerite.

(2) Pb-Zn preferential flotation or mixed-preferential flotation

The content of lead in lead-zinc ore is usually less than that of zinc, and the floatability of lead is generally better than that of zinc, but it is difficult to activate after the lead ore is inhibited. The flotation process usually has two methods: preferential flotation and mixed-preferential flotation.

Among them, there are many applications of priority flotation, because it has a simple process structure and does not require chemical removal operations. It is mainly suitable for ore with simple ore material composition and coarse mineral distribution; more suitable for medium and small lead-zinc concentrators.

The mixed concentrate must be removed before flotation and separation, and the commonly used methods of chemical removal are: activated carbon, sodium sulfide and mechanical stirring methods. The main disadvantage of this method is that the process is more complicated.

For coarse, medium and fine unevenly embedded lead-zinc sulfide minerals, extremely complex technological processes such as coarse concentrate, medium ore, tailings regrinding and gravity separation, as well as this section of grinding and this section of flotation can be used.

For lead-zinc sulfide minerals that are embedded in fine-grained or coarse-grained aggregates, and the surrounding rock is less mineralized, heavy media or other beneficiation methods can be used for pre-selection after rough grinding, and part of the tailings are thrown away, and then lead and zinc are directly or regrind. Flotation separation, which can reduce the production cost of beneficiation, increase the processing capacity, and increase economic benefits.

02 Cu-Pb-Zn-Fe Flotation

In the polymetallic copper-lead-zinc-iron sulfide ore, the content of pyrite and pyrrhotite is generally high. Because of their good floatability, the quality of the concentrate will be affected during flotation separation, and they are low Valence minerals, therefore, must be suppressed. Pyrite and pyrrhotite are the main raw materials for the sulfuric acid industry, and they are usually recovered. Pyrrhotite has high magnetic properties and can be processed by magnetic separation or flotation.

 Understanding Flotation Methods for Polymetallic Sulfide Ore Equipment production procurement suppliers flotation machines polymetallic ores sulfide equipment applications 第3张

(Flotation cell is deliveried to Cu-Pb-Zn-Fe plant)

(1) Cu preferential flotation or mixing - preferential flotation

The copper-sulfur ore adopts the flotation separation process with priority and mixed-priority flotation process as the main process. For some ores with complex properties, this section of grinding, this section of selection, separate treatment of medium ore, and separation of mud and sand are used.

Since copper sulfide minerals and pyrite have good floatability, the content of copper sulfide minerals in copper sulfide ore is less than that of pyrite, and pyrite is a low-priced mineral. Therefore, copper flow flotation Separation is often widely used lime method to inhibit pyrite, flotation of copper sulfide minerals. The floatability of pyrite in some copper-sulfur ores is good, and it is difficult to suppress it with a single lime, and a combination of inhibitors must be used to strengthen the suppression of pyrite.

(2) Pb mixed flotation

In the lead-zinc-sulfur polymetallic sulfide ore, if the floatability of galena and pyrite is better than that of sphalerite, mixed flotation of lead-sulfur is used to suppress zinc. The lead-sulfur mixed concentrate is then used to suppress sulfur and float lead; if the flotability of galena, pyrite and part of sphalerite in the ore is good, mixed flotation is used to select lead, zinc and sulfur, and then The lead-zinc-sulfur mixed concentrate uses lime to suppress zinc-sulfur floating lead, and then lime is used to suppress sulfur-floating zinc.

(3) Zn preferential flotation

Zinc-sulfur ore is relatively rare. In lead-zinc-sulfur, copper-zinc-sulfur, copper-lead-zinc-sulfur and other polymetallic sulfide ores, copper and lead sulfide minerals are usually preferentially flotated to suppress zinc sulfide minerals. In the separation of zinc and sulfur, although the natural floatability of pyrite is better than that of sphalerite, its content is high because it is a low-priced mineral. Lime method is often used to suppress sulfur floating zinc, and copper sulfate is added to activate zinc minerals. Because lime causes strong alkalinity (pH=10.5-12), pyrite is strongly inhibited. At this time, copper sulfate has the best effect of activating sphalerite. Therefore, the floatability of zinc and sulfur occurs. The difference is convenient for flotation separation.

03 Cu-Pb Flotation

In the beneficiation process of polymetallic copper-lead-zinc sulfide ore, copper-lead mixed flotation is often used to obtain mixed concentrate. There are a lot of excess flotation reagents on the surface of copper and lead minerals and in the pulp, which often have a great impact on flotation separation. Therefore, before separation, the chemical on the mineral surface and in the pulp must be removed first. In production practice, sodium sulfide and activated carbon are commonly used to remove remained reagent.

(1) Cu-Pb Priority Flotation

In the copper-lead mixed concentrate, the lead sulfide minerals are mainly galena, and there are many kinds of copper sulfide minerals, and their properties and floatability are different. Therefore, the copper-lead flotation separation process is often complicated, and there are many influencing factors. The copper-lead flotation separation process mainly includes: suppressing lead and floating copper; suppressing copper and floating lead; suppressing copper and floating lead - suppressing lead and floating copper.

04 Cu-Mo Flotation

Copper-molybdenum sulfide ore is mainly composed of bauxite, chalcopyrite and chalcocite, which is one of the main sources of molybdenum concentrate. There are three main separation schemes for the flotation of copper molybdenum ore:

(1) Cu-Mo mixed flotation

Mixed flotation to obtain copper-molybdenum mixed concentrate, and then flotation to separate copper concentrate and molybdenum concentrate. This method is the most widely used.

(2) Mo-Cu preferential flotation

When the molybdenum content in the ore is higher than 0.06%, the method of flotation of molybdenum first and then copper floatation can be adopted.

(3) Cu-Mo priority flotation

When the content of sulfide minerals in the ore is very small, the method of preferentially flotation of copper and then flotation of molybdenum can be adopted. But in actual production, this method is rarely used. In preferential flotation, it is often uneconomical to suppress molybdenum and float copper. For this reason, mixed flotation should be widely used to obtain copper-molybdenum mixed concentrates in the case of rough grinding as much as possible, and the total recovery rate of the two should be the highest. Then the mixed concentrate is reground to make the copper and molybdenum sulfide minerals fully dissociated and then separated by flotation.

 Understanding Flotation Methods for Polymetallic Sulfide Ore Equipment production procurement suppliers flotation machines polymetallic ores sulfide equipment applications 第4张

(Flotation cell for copper-molybdenum separation)

05 Cu-Ni Flotation

The mixed flotation method is commonly used in the flotation separation of copper-nickel sulfide ore, and then the copper-nickel mixed concentrate is separated by the method of suppressing nickel and floating copper, so that a large amount of tailings can be thrown away, which is economically reasonable. According to the properties of copper-nickel sulfide ore and the requirements for concentrate products, the flotation separation process of copper-nickel sulfide ore usually mainly includes full separation and semi-separation.

(1) Cu-Ni mixed flotation

In the copper-nickel sulfide ore, because most of the copper minerals and nickel minerals have a less close symbiotic relationship, there is a certain difference in the floatability between them. The mixed concentrate is obtained by mixed flotation, and then the mixed concentrate is separated. , can obtain copper concentrate with copper content of 25%~30%, nickel content less than 2% and nickel concentrate with nickel content higher than 8%, only by adopting full separation. Such copper and nickel concentrate smelting treatment is more economical.

(2) Cu-Ni mixed flotation-smelting semi-separation

In copper-nickel sulfide ore, copper and nickel minerals are embedded with fine particle size, close symbiotic relationship, and complex mineral composition, including gangue minerals that are easy to float. Concentrates (containing 25%~30% copper) can only get copper-nickel mixed concentrates, which are semi-separated. Its products are smelted into high nickel matte, and then the copper-nickel flotation separation is carried out. When the copper-nickel concentrate is separated by flotation, because the floatability of copper sulfide is better than that of nickel ore, the process of suppressing nickel floating copper is often used.

Therefore, in the production practice of beneficiation, for the easy beneficiation, mixed flotation is often used, and then the separation is carried out. However, for those refractory ores with a large degree of alteration, it is generally not suitable to use the full separation process. The main reason is that the refractory ores contain a large amount of gangue minerals that are easy to float. The minerals float together, thereby reducing the grade of the copper concentrate.

06 Cu-Fe Flotation

In the beneficiation of copper and iron ore, the combined flotation-magnetic separation process is often used. First flotation of copper minerals, then magnetic separation of iron minerals, the quality of iron concentrates can be easily guaranteed. There are some differences in beneficiation methods according to the content of associated elements in the ore:

(1) Cu single flotation

When the ore is low in sulfur, copper flotation is the same as for single copper sulfide minerals.

(2) Cu-Fe priority - mixed flotation

For copper and iron ore with more iron sulfide minerals, priority and mixed flotation process are generally used, and the lime method is usually used to suppress floating copper. If the ore contains more pyrrhotite, the iron concentrate needs to be desulfurized. When the ore contains high cobalt, cobalt is generally enriched in sulfur concentrate, which can be sold as cobalt concentrate. When the ore contains high molybdenum, molybdenum is generally enriched in copper concentrate, and copper-molybdenum separation and flotation can be carried out to recover molybdenum.

(3) Cu-Fe flotation-gravity separation

The iron minerals in the copper-iron ore are mainly hematite, which can be separated by a combined flotation-gravity separation process.

 Understanding Flotation Methods for Polymetallic Sulfide Ore Equipment production procurement suppliers flotation machines polymetallic ores sulfide equipment applications 第5张


(Flotation cell for Cu-Fe sulfide ore separation)

07To Wrap Up

The above is an introduction to the flotation methods of copper-lead-zinc sulfide ore, copper-lead-zinc-iron sulfide ore, copper-molybdenum sulfide ore, copper-nickel sulfide ore and copper-iron sulfide ore. The next article will continue to introduce the flotation method of antimony-mercury sulfide ore, antimony-gold sulfide ore, tin-bearing polymetallic ore, tungsten-bearing polymetallic sulfide ore and gold-bearing polymetallic sulfide ore to you. Please click what are flotation methods for polymetallic sulfide ore ii for more details.


Leave a message with your needs or comments

Add comment:

WeChat

+86 18092529083Scan QR code8618092529083